What are the common problems in HASL (hot air solder leveling) for rigid PCBs?
Uneven solder on pads, insufficient via soldering, uneven surface. Control solder
What is the minimum green oil bridge width for rigid PCBs?
Conventional: 0.1mm. High-density boards with LDI: 0.075mm, preventing soldering bridging.
How does copper foil thickness affect heat dissipation in rigid PCBs?
Each 1oz (35μm) increase raises thermal conductivity by 38%. 3oz foil in high-power applications reduces temperature rise by 15%-20% with thermal vias.
What are the advantages and disadvantages of flying probe and bed-of-nails testing for rigid PCBs?
Flying probe: Coverage >98%, suitable for small batches/high density, slow (3-5s/point). Bed-of-nails: Fast (<1s/point), high cost, coverage 85%-95%, suitable for mass production.
What is the difference between blind and buried via fabrication processes in rigid PCBs?
Blind vias: Laser/mechanical drilling + plating, depth ≤0.5mm, for surface interconnection. Buried vias: Mechanical drilling + lamination, requiring alignment, for inner-layer signals to reduce parasitic parameters.
What is the surface insulation resistance (SIR) requirement for rigid PCBs?
Per IPC-TM-650, ≥10¹⁰Ω after 168h at 85℃/85% RH, ≥10¹²Ω for high-end applications, requiring surface cleanliness control.
What are the causes and solutions for deformation during reflow soldering of rigid PCBs?
Causes: CTE mismatch, uneven thickness, improper temperature curve. Solutions: Select CTE ≤15ppm/℃ materials, control thickness tolerance ±0.05mm, optimize heating rate ≤3℃/s.
What does the design for manufacturability (DFM) of rigid PCBs mainly check?
Minimum line width/spacing, hole diameter/pad ratio (pad ≥hole +0.4mm when hole ≥0.3mm), copper area ratio (30%-70%), drill aspect ratio (≤8:1), solder mask bridge width (≥0.1mm).
What is the withstand voltage standard for rigid PCBs?
Per UL 796, FR-4 material ≥1400V/mm at 25℃/50% RH. Creepage distance 1mm corresponds to 100-200V.
What is the impedance control accuracy requirement for rigid PCBs?
General: single-ended ±10%, differential ±8%. High-speed (>1Gbps): single-ended ±5%, differential ±3%, adjusted via line width, dielectric thickness, copper thickness.
How to remove burrs from drilled holes in rigid PCBs?
Deburring machine brushing (pressure 0.3-0.5MPa, speed 2-3m/min). Chemical micro-etching (sodium persulfate 100-150g/L, 40-50℃, 1-2min).
How does copper foil roughness affect signal transmission in rigid PCBs?
Higher roughness enhances skin effect and signal loss. RTF foil Ra<0.5μm (suitable for high frequency >10GHz). VLP foil Ra<0.3μm (loss reduction 15%-20%).