PCB & PCBA Frequently Asked Questions

PCB & PCBA Frequently Asked Questions

A centralized engineering knowledge base addressing common questions across PCB manufacturing, PCBA assembly, materials, processes, and reliability-driven design decisions.

PCB Manufacturing FAQ

How to handle moisture in rigid PCBs?

Per IPC-J-STD-033, bake at 125℃ for 4-8h (≤1.6mm: 4h, >1.6mm: 8h) to reduce moisture content below 0.1%.

How to choose between via covering and plugging in rigid PCB design?

For conductivity, choose resin plugging (depth ≥80% via depth, flatness error ≤10μm). For insulation only, choose covering (coverage width ≥0.1mm).

What is the minimum line width/spacing for rigid PCBs?

Conventional: 6/6mil (0.1524mm). LDI + chemical etching: 3/3mil (0.0762mm). HDI boards: 1/1mil (0.0254mm).

What is the general thickness of the solder mask for rigid PCBs?

Conventional: 15-30μm (IPC-6012), dense areas ≥20μm. Screen printing: 20-25μm, light curing: 15-20μm.

What is the optimal temperature curve for wave soldering of rigid PCBs?

Preheat: 90-130℃ (60-120s). Soldering zone: 240-260℃ (contact 2-4s). Cooling rate: 3-6℃/s (J-STD-003).

How to test the via copper thickness of rigid PCBs?

Metallographic sectioning (IPC-TM-650, through-hole ≥20μm, blind/buried via ≥18μm). XRF non-destructive testing (accuracy ±0.5μm).

What is the bending strength standard for rigid PCBs?

FR-4 material: longitudinal ≥345MPa, transverse ≥276MPa (ASTM D790). 1.6mm thickness ≥300MPa.

What is the interlayer alignment requirement for multilayer rigid PCBs?

Per IPC-6012, general multilayer boards ≤75μm, HDI boards ≤50μm. Laser drilling positioning accuracy ±25μm, controlled with high-precision exposure machines.

How to solve etching defects in rigid PCB manufacturing?

Adjust solution concentration (acidic etchant: CuCl₂ 180-220g/L, HCl 1.0-1.5mol/L), temperature 50-55℃. For excessive under-etching, reduce speed and increase spray pressure to 2-3bar.

How to select surface finishing processes for rigid PCBs?

Per IPC-4552, ENIG suits high-frequency/high-reliability (Ni: 3-5μm, Au: 0.05-0.1μm). OSP is low-cost (film thickness: 0.2-0.5μm, suitable for short-term storage). HASL is mature (Sn thickness >2.5μm, poor flatness).

How to test the mechanical properties of rigid PCBs?

Bend test (observe cracks at specified angles/cycles). Drop test (simulate impacts). Vibration test (simulate vibrations to check soldering and structure).

What is the principle and application scenario of AOI (Automated Optical Inspection)?

Collect images via optical cameras and compare with standards to detect defects like missing components, misalignment, shorts. Applied in real-time inspection after printing, placement, reflow soldering to improve efficiency and quality.