PCB & PCBA Frequently Asked Questions

PCB & PCBA Frequently Asked Questions

A centralized engineering knowledge base addressing common questions across PCB manufacturing, PCBA assembly, materials, processes, and reliability-driven design decisions.

PCBA Process Flow FAQ

What is the impact of component placement angle deviation on soldering?

An angle deviation > 5° may cause the misalignment of leads/solder balls and pads, increasing the risk of bridging or false soldering. It needs to be compensated and corrected through equipment software.

What is the "first - piece three - inspection" process for component placement offset exceeding standards?

Operator self - inspection → Team leader re - inspection → Quality inspector sampling inspection. Mass production is allowed only after confirmation.

How is the "rejection rate" standard set for component tape packaging?

For components of 0402 and above, the rejection rate should be ≤0.5%; for micro - components of 0201 and below, the rejection rate should be ≤1.5%.

What additional FDA certification requirements must be met for PCB placement in medical devices?

① Each batch of components needs to provide a bill of materials (BOM); ② The operator ID and operation time need to be recorded during the placement process; ③ Solder joints need to be 100% X - Ray inspected and the image records need to be saved.

What special requirements does selective wave soldering have for component placement layout?

① Reserve a process edge of ≥5mm for fixture clamping; ② The spacing between adjacent components should be ≥3mm to avoid interference during tin - spraying.

What are the advantages of virtual commissioning in new machine model introduction?

① Verify program logic in advance (reducing on - site debugging time by 50%); ② Simulate extreme working conditions to test equipment stability; ③ Train operators without occupying actual equipment.

What is the impact of lead - free solder application on placement energy consumption and corresponding countermeasures?

Lead - free solder has a high melting point (about 217℃), resulting in a 15 - 20% increase in reflow soldering energy consumption. Energy consumption can be reduced by optimizing the furnace temperature curve (such as shortening the holding time).

What is the requirement for component placement window time with lead - free solder paste (Sn - Ag - Cu)?

The interval from printing to placement needs to be ≤1 hour to avoid solder paste absorbing moisture and causing reflow soldering voids.

What fire prevention measures are required for placing flammable components (e.g., solvent - containing packages)?

An inert gas fire - extinguishing system needs to be equipped, and the oxygen concentration in the workshop needs to be controlled between 18 - 21%.

How to connect placement equipment to the Industrial Internet of Things (IIoT)?

① Add edge computing modules (such as PLC gateways); ② Use the OPC UA protocol to achieve communication between devices; ③ Establish a data hub to store real - time production data.

How to reduce the environmental impact of nozzle wear in the placement process?

① Use ceramic or cemented carbide nozzles (lifetime increased by 3 - 5 times); ② Establish a nozzle refurbishment process (such as laser - repairing the worn surface).

What core skills should placement engineers master?

① Equipment principles and programming (such as G - code, teach - pendant programming); ② Process parameter optimization (such as pressure, temperature curves); ③ Fault diagnosis and preventive maintenance; ④ Application of quality tools (such as SPC, FMEA).