PCB & PCBA Frequently Asked Questions

PCB & PCBA Frequently Asked Questions

A centralized engineering knowledge base addressing common questions across PCB manufacturing, PCBA assembly, materials, processes, and reliability-driven design decisions.

PCBA Basics & Overview

What are the typical alloy compositions and melting points of lead-free solder pastes?

Dominant SAC305 (96.5Sn/3.0Ag/0.5Cu) melts at 217℃, 34℃ higher than Sn-Pb eutectic (183℃), requiring higher reflow temperatures.

How to design pad sizes for component packages?

Follow IPC-7351: QFP pad width +0.1-0.2mm vs. lead width; 0603 pads recommend 0.65×0.65mm for 0.04-0.06mg solder paste per pad.

What is the process limit for minimum line width/spacing?

Standard SMT: 4/4mil (0.1/0.1mm); HDI processes achieve 2/2mil (0.05/0.05mm) with high-precision exposure and electroless copper plating.

How does Tg value of PCB substrate affect assembly processes?

Tg value determines substrate heat resistance. Standard FR-4 has Tg ~130-140℃, while high-Tg (≥170℃) materials withstand reflow peaks of 250℃, reducing delamination risk. Lead-free processes require Tg≥150℃.

What are the roles of flux and how to choose?

Roles: Remove oxides, reduce surface tension, improve wettability. Types: Inorganic (high activity, corrosive, requires cleaning), organic (moderate activity, low corrosion, requires cleaning), rosin-based (common, non-corrosive, no-clean). Choose by process and product

What are common solder defects and solutions?

Dry joint: Adjust temperature, extend time, clean surfaces; Short circuit: Reduce solder, optimize design; Bridging: Adjust paste volume, temperature profile; Insufficient solder: Increase paste, optimize process; Rough solder: Add flux, adjust temperature.

How to ensure soldering quality?

Control process parameters (temperature profile, soldering time), calibrate equipment, train personnel, use qualified materials, AOI/X-Ray inspection, and timely rework of defects.

What are the requirements for solder selection?

Select by process: Lead-free solder paste (Sn-Ag-Cu, 217-227℃) for reflow; leaded/lead-free solder bars (Sn-Pb, 183℃ for leaded) for wave soldering; solder wire for manual soldering, considering wettability and cost.

When is manual soldering used and its precautions?

Applications: Prototyping, repair, and hard-to-reach areas for automation. Precautions: Soldering iron 20-60W, solder wire 0.5-1.0mm, temperature 300-350℃, time 3-5s, pre-cleaning, and post-inspection.

What is wave soldering principle and suitable components?

Principle: Liquid solder forms a wave, and PCB leads are soldered when passing through. Suitable for through-hole and large SMT components.

What is reflow soldering principle and temperature profile?

Principle: Solder paste printing → component placement → heating to melt paste → cooling to solder. Temperature profile: Preheat (1-3℃/s to 150-180℃), soak (180-200℃, 60-120s), reflow (peak 217-235℃, 30-90s), cool (3-6℃/s).

What environmental requirements do high-precision components have?

Requires controlled temperature/humidity (±2℃, 40%-60%RH) and ESD protection (anti-static flooring, wrist straps, work clothes) to avoid parameter drift and ESD damage.